简体中文 / English
Hydrophiling Treatment Agent
Hydrophiling Treatment Agent
Product Introduction:
This series are used in the production of air-conditioner’s cooling fin for the hydrophilization of aluminum foil. The treated aluminum foil offers a lasting hydrophilia and odor-resistance.
........................................................................................................................................................................

Product model:

Hydrophiling treatment agent


Product Model

Product Property

Substrate

Usage

Performance Feature

FY-AlCOAT-450

Waterborne organic system

 

Aluminum foil

Applied with roller coating technique , and dried for 20 seconds in the temperature of 220 to 260℃.

It is used in the cooling fin of air-conditioner. The treatment offers a lasting hydrophilia and odor-resistance.

FY-AlCOAT-650

Organic / inorganic compound waterborne system

Aluminum foil

Applied with roller coating technique , and dried for 20 seconds in the temperature of 220 to 260℃.

It is used in the cooling fin of air-conditioner. The treatment offers a lasting hydrophilia and odor-resistance.

FY-AlCoat-252

Organic / inorganic compound waterborne system

Aluminum foil

Applied with roller coating technique , and dried for 20 seconds in the temperature of 100 to 140℃.

It is used as the primer paint for hydrophilic aluminum foil, to enhance the corrosion-resistance of base materials.

FY-AlCoat-200

Organic / inorganic compound system

Cooling fin

Impregnated after being diluted to 28%, and dried for 20 min in the temperature of 170 to 190℃.

It is used as the hydrophiling treatment agent for the cooling fin of auto air-conditioner.



Relevant pictures:
 

上一件: Passivant for Cold-rolled Galvanized Steel Sheet
下一件: Insulating Treatment Agent for Silicon Steel
 
Copyright© 2008 -2018Shanghai Fengye Surface Treatment Agent Co., Ltd. All Rights Reserved
Add:No. 170 Jinfeng Road, Pudong New Area, Shanghai   Tel:021-58585844